Technical parameters:
Chemical Composition | C | Si | Mn | P | S | Cr | Mo | Ni | V | N |
0.16-0.25 | ≤1.0 | ≤1.0 | ≤0.04 | ≤0.03 | 12.0-14.0 | / | ≤1.0 | / | / | |
ASTMF899-12B |
Basic information:
420A-1.4021 is a modified martensitic stainless steel with a complex smelting process of EAF+VOD and a low carbon content.
It is usually used for the cutting edges of most common medical devices.
Applicable standards:
Europe | USA | Other |
1.4021 | AISI420 |
Medical applicable standards: ASTMF899-12B
Basic parameters:
UTS (Mpa) | 0.2%YS (Mpa) | A% | Z% | Hardness (HRC) | |
Annealed | 20.0 | ||||
Quench+temper | 46-50 |
Medical applicable product range:
Hardness requirements (46-50HRC), products with balanced wear resistance and corrosion resistance.